Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kraton D1111 KSM - TPS - Kraton Polymers

Material Data Center offers the following functions for Kraton D1111 KSM:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kraton D datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
Kraton D1111 K is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%.
Kraton D1111 KSM - supplied as a dusted powder.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 2 g/10min ASTM D 1238
温度 200 °C -
荷重 5 kg -
機械的特性単位テスト基準
ASTM数据
伸び率300%弾性率 1.38 MPa ASTM D 412
ショア硬さA 45 - ASTM D 2240
引張強度 20 MPa ASTM D 412
破断伸び 1200 % ASTM D 412
その他の特性.単位テスト基準
Other Standards[S]
密度 930 kg/m³ ASTM D 4025
S: These properties are reported by the producer according standards that are different to our defaults.
特殊な特性
成形加工法.
コーティング.
納入形状.
パウダー.
特殊な特性.
透明.
な特性
Copolymer
耐薬品性
Oxidation Resistance
領域別の利用可能性
北アメリカ., ヨーロッパ., アジア/太平洋地域., 近東/アフリカ
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.